    Specifications
    HS Code 965283
    Density 1.24-1.25 g/cm³
    Melt Flow Rate 10-30 g/10 min (190°C/2.16 kg)
    Tensile Strength 50-60 MPa
    Elongation At Break 3-5%
    Flexural Strength 80-90 MPa
    Flexural Modulus 3000-3500 MPa
    Notched Izod Impact Strength 2-4 kJ/m²
    Heat Deflection Temperature 90-100°C
    Vicat Softening Temperature 100-120°C
    Glass Transition Temperature 55-60°C
    Melting Temperature 150-170°C
    Water Absorption <0.5%
    Molding Shrinkage 0.3-0.8%
    Biobased Carbon Content ~100%
    Biodegradability Industrial compostable
    Appearance Natural/off-white pellets
    Processing Temperature 190-220°C
    Drying Temperature 80°C
    Drying Time 2-4 hours
    Mold Temperature 20-40°C

    As an accredited Polylactic Acid REVODE711H factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Polylactic Acid REVODE711H is supplied in 25 kg net-weight, moisture-resistant paper bags, palletized and shrink-wrapped for industrial transport.
    Container Loading (20′ FCL) Polylactic Acid REVODE711H loaded in 20′ FCL: palletized bags, moisture protection, even weight distribution, and secure bracing for transport.
    Shipping Polylactic Acid REVODE711H ships as a non-hazardous, non-regulated solid polymer. Use moisture-barrier bags, fiber drums, or lined cartons on pallets. No UN number, hazard class, or special transport label required. Keep dry, cool, and away from direct sunlight, heat, and contamination. Follow local regulations.
    Storage Store Polylactic Acid REVODE711H in a cool, dry, well-ventilated area. Keep containers tightly closed in original packaging. Protect from moisture, humid air, direct sunlight, heat, and ignition sources. Avoid prolonged storage above ambient temperatures. Maintain clean, segregated storage away from incompatible materials. Do not expose to open flames. Follow supplier SDS and use first-in, first-out stock rotation.
    Shelf Life Polylactic Acid REVODE711H: typically 24 months shelf life if stored sealed, cool, dry, away from moisture, heat, and sunlight.
    Application of Polylactic Acid REVODE711H

    When REVODE711H is specified for single-use foodservice cutlery, the production window is controlled less by plastication temperature than by residual moisture management and cooling-rate-directed crystallinity. Desiccant-wheel drying with a hopper inlet dew point no higher than -40 °C and a polymer temperature of 80 °C for 4–6 h lowers pellet moisture from typical inbound values of 0.2–0.5 wt% to below 250 ppm; above that threshold, hydrolytic chain scission can shift the melt flow rate measured under ISO 1133-1:2022 at 210 °C and 2.16 kg by more than 4 g/10 min within 30 min of residence time at 185 °C. Injection moulding on reciprocating-screw machines with 20:1–24:1 L/D and a compression ratio of 2.0:1–2.5:1 is set to a barrel profile of 165 °C rear, 175 °C middle, 190 °C front, and 185 °C nozzle, while the mould surface is held between 20 °C and 60 °C; higher mould temperatures extend cycle time beyond 45 s on 16-cavity cutlery tooling but reduce warpage in forks with a length exceeding 160 mm. The addition ratio for masterbatch in cutlery is normally 2–4 wt% of a temperature-stable colour concentrate, with 0.25–0.50 wt% of an inorganic nucleating agent added only where demoulding is impaired by low crystallinity; higher nucleant loadings reduce transparency to a level that is measurable as a haze increase and are therefore avoided in clear examples. Compliance for food-contact cutlery distributed in the EU is assessed under Regulation (EU) No 10/2011, Annex I, with an overall migration limit of 10 mg/dm² into food simulant B for acidic aqueous foods and food simulant D2 for fatty foods, while U.S. importers typically rely on 21 CFR 174.5 general provisions for indirect food additives and the resin supplier’s food-contact notification for the specific polymerisation formulation. Compostability claims for the finished article require EN 13432:2000 or ASTM D6400-23, including disintegration according to ISO 20200 and ecotoxicity testing; industrial compostability is not equivalent to home compostability at temperatures below 40 °C. Finished terminal product types are injection-moulded knives, forks, spoons, sporks, and sampling stirrers; these articles are ejected from multi-cavity families with hot-tip gating and are typically packed immediately after edge inspection because residual heat above 30 °C can cause surface blocking.

    Does Melt Strength Limit Thermoforming of Clear Deli and Produce Containers from REVODE711H?

    Melt strength rather than melt flow is the governing variable when the resin is converted into a continuous sheet and then reheated into a female mould. On single-screw extruders with grooved feed sections and 30:1–36:1 L/D, the sheet line runs a descending temperature profile of 175 °C at the feed throat rising to 210 °C at the adapter, with a melt pump maintaining pressure at 8–12 MPa before the coat-hanger die. The addition ratio for a thermoforming-grade compound typically includes 0.2–0.6 wt% nucleating agent to raise cold crystallisation rate, 0.1–0.5 phr chain extender to build branched-chain entanglement, and 0.5–1.0 wt% antiblock masterbatch to prevent roll stacking adhesion; the chain extender must be pre-dispersed in a co-rotating twin-screw extruder with 44:1 L/D before sheet extrusion because direct metering causes localised gel formation. The downstream process requires a polished three-roll calendar stack with roll temperatures of 40 °C, 55 °C, and 30 °C from first nip to third roll; sheet thickness is controlled to 0.30–0.80 mm with a target variation of ±0.03 mm across the web. Thermoforming into clamshell cavities uses infrared-quartz heating to a sheet surface temperature of 70–90 °C; below 68 °C the sheet tears at draw ratios above 3:1, while above 95 °C surface tack blocks plug-assisted pre-stretch. The mould is temperature-controlled at 20–25 °C and trimmed with steel-rule dies after ejection. EU food-contact compliance is again under Regulation (EU) No 10/2011; overall migration testing is conducted for the final thermoformed article under the intended use and worst-case surface-to-volume ratio, and U.S. compliance is verified through 21 CFR 174.5. Compostability labelling uses EN 13432:2000 or ASTM D6400-23. Terminal finished product types are clear hinged clamshells for deli salads, produce packs, bakery trays, cup lids, and egg carton inserts; the sheet scrap generated during trimming is 20–30 wt% of input and can be reground into the sheet line at 10–20 wt% only after flake drying at 60 °C for 2 h, beyond which MFR drift causes gauge variability.

    Compliance verification matrix for REVODE711H food-contact and end-of-life claims
    ScenarioStandard or regulationTest method or clauseRequired result
    Foodservice cutlery and thermoformed food packagingRegulation (EU) No 10/2011Annex III and IV overall migration10 mg/dm² maximum
    Foodservice cutlery and thermoformed food packaging21 CFR 174.5Indirect food additive general provisionsNo adulteration or migration above threshold
    Compostability claimsEN 13432:2000ISO 20200 disintegration; OECD 208 ecotoxicity90% disintegration in 12 weeks; no ecotoxicity
    Compostability claims, U.S.ASTM D6400-23ASTM D5338-15 biodegradation90% mineralisation within 180 days
    3D printing filament restricted substancesEU RoHS Directive 2011/65/EUIEC 62321 screeningPb 1000 ppm; Hg 1000 ppm; Cd 100 ppm
    3D printing filament SVHCREACH Regulation (EC) No 1907/2006Article 33 notificationSVHC below 0.1 wt%

    In filament extrusion for fused filament fabrication, REVODE711H is compounded with 0.5–3.0 wt% pigment masterbatch and 0.1–0.5 wt% of a non-migrating processing lubricant to maintain consistent feeding into a single-screw filament line; 0.1–0.3 wt% of a nucleating agent is added only when the finished filament must survive spooling at a diameter of 1.75 mm without breakage during fast retraction. Compliance for the compounded pellet and filament is documented under EU REACH Regulation (EC) No 1907/2006 for SVHC content and EU RoHS Directive 2011/65/EU for lead, mercury, cadmium, hexavalent chromium, PBB, and PBDE, with X-ray fluorescence screening on incoming pigment batches because colourants are the dominant source of restricted heavy metals. The downstream production process uses a co-rotating twin-screw extruder with 40:1–44:1 L/D for the initial dispersion step at 165–185 °C, a water strand bath held at 35–45 °C, and a strand pelletiser producing 2.5 mm cylindrical granules; the drying step before filament extrusion is 80 °C for 4 h to below 250 ppm moisture. The filament line itself uses a barrier screw with 25:1 L/D, a melt pump, and a die land length-to-diameter ratio of 10:1; diameter is measured by dual-axis laser micrometers and controlled by adjusting haul-off speed to maintain 1.75 mm ± 0.05 mm or 2.85 mm ± 0.10 mm. Finished product types are spooled PLA monofilaments for fused filament fabrication in desktop and industrial printers; the spool core is sized to prevent curvature-induced fracture when the filament is stored below 50% RH because PLA embrittlement increases as moisture uptake exceeds 0.5 wt%.

    Cosmetic Packaging Moulding Conditions and Surface Replication Limits

    The injection moulding of jars, closures, and compact housings in REVODE711H is constrained by a replication threshold: a cavity surface polished to SPI-A2 does not replicate completely when the mould temperature remains below 35 °C, whereas raising the mould to 45 °C increases gloss to a measured 85 GU at 60° on a glossmeter but extends cooling time by 6–10 s per wall thickness of 2 mm. The addition ratio for a cosmetic-grade compound is 1–3 wt% of a high-opacity masterbatch and 0.5–1.0 wt% of an internal slip and anti-scratch additive, with the slip additive limited to 1.0 wt% because migration to the seal area reduces cap torque retention. Barrel temperatures are 175 °C, 185 °C, 190 °C, and 185 °C nozzle, and the injection speed is profiled from 30 mm/s for the gate area to 80 mm/s for the main fill to prevent jetting. Regulatory testing for the finished article addresses EU Regulation (EC) No 1223/2009 Annex II restricted substances in the cosmetic product-contact surface, REACH Regulation (EC) No 1907/2006 Annex XVII restrictions on phthalates and polycyclic aromatic hydrocarbons, and EN 13432:2000 if the brand claims industrial compostability. Terminal finished articles are single-wall jars with a wall thickness of 1.5–2.5 mm, snap-fit compacts, and threaded closures with a torque retention target of 0.8–1.2 N·m after the first opening; the closures are moulded as two-piece assemblies and tested for dimensional stability under ISO 294-4:2018 shrinkage measurements.

    The Crystallisation Retardation Window in Horticultural Clip and Plant Tag Moulding

    The use of REVODE711H in greenhouse clips and plant-tag applications operates inside a narrow crystallisation window because the part must be ejected at low cycle times but must not embrittle during field installation. The addition ratio for a mineral-reinforced horticultural compound is 5–10 wt% talc or calcium carbonate masterbatch to raise flexural modulus above 3.0 GPa under ISO 178:2019, while colour concentrate is added at 2–4 wt%; loadings above 12 wt% filler cause notched Izod impact values measured under ISO 180:2023 to fall below 2.0 kJ/m², which results in clip failure during insertion onto 6–8 mm vine stems. Processing on a standard injection moulding machine uses barrel temperatures from 160 °C to 185 °C and a chilled mould surface of 15–25 °C; the fast cooling produces cycle times of 28–38 s on 8-cavity tooling but leaves residual internal stress that must be measured by polarised-light inspection for tags longer than 100 mm. Compliance for compostability claims follows EN 13432:2000, with disintegration measured by ISO 16929:2021 and ecotoxicity by OECD 208; products intended for outdoor use require a separate UV-stabilised masterbatch because unstabilised PLA loses tensile strength under QUV exposure, and published data for multi-year outdoor ageing of this specific grade is limited, so accelerated laboratory results should not be extrapolated to field service life claims. Terminal finished product types are plant identification tags, vine clips, seedling clips, and greenhouse row markers, all of which are marked with lot codes to trace the filler masterbatch used.

    Free Quote

    Competitive Polylactic Acid REVODE711H prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@bouling-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@bouling-chem.com

    Inquiry

    Get Free Quote of Zhejiang Hisun Biomaterials Co., Ltd

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    For extrusion-dominated converting routes—sheet extrusion, cast film, and inline thermoforming—Polylactic Acid REVODE711H is a semicrystalline poly(L-lactic acid) (PLLA) resin supplied in pellet form under the REVODE 700-series designation. The grade is positioned within the REVODE portfolio for processes that require lower melt flow rate and higher melt strength relative to high-speed injection moulding. Publicly available grade-specific datasheets for REVODE711H are limited; therefore, melt flow rate, D-lactic acid content, and crystallinity must be verified against the manufacturer’s certificate of analysis before process parameters are fixed. The table below defines the specification verification matrix for incoming material control. The subsequent sections define the technical envelope that distinguishes REVODE711H from unmodified injection moulding PLA and from impact-modified compounds.

    Specification parameterTest methodData source / verification condition
    Melt mass-flow rateISO 1133-1:2022Lot certificate of analysis; verify at 210 °C, 2.16 kg
    DensityISO 1183-1:2019Lot certificate of analysis; immersion method
    Tensile strength at yield, elongation at breakISO 527-2:2012Lot certificate of analysis; type 1A specimen
    Flexural modulusISO 178:2019Lot certificate of analysis
    Notched Izod impactISO 180:2019Lot certificate of analysis; 80 mm × 10 mm × 4 mm specimen
    Heat distortion temperatureISO 75-2:2020 method BLot certificate of analysis or finished-article test

    What Limits High-Shear Extrusion of REVODE711H When Moisture Exceeds 250 ppm?

    Hydrolytic chain scission is the dominant degradation route in PLA extrusion. When pellet moisture exceeds 250 ppm, the combination of residual water and melt temperatures above 180 °C cleaves ester linkages, reducing molecular weight and melt strength within the first residence-time distribution. The molecular weight loss is autocatalytic because carboxylic acid end groups further catalyze hydrolysis; this is why deep drying is non-negotiable. A desiccant dryer with an air dew point not exceeding -40 °C and an air temperature of 80–85 °C is standard for virgin REVODE711H; residence time of 4–6 h in the drying hopper is normally sufficient. For regrind fractions above 30 wt%, drying time is extended to 6–8 h because ground flake has higher surface area and adsorbs moisture during granulation. Dried pellets are transferred by vacuum loaders with closed-loop dry-air purging; open augers or ambient-air hoppers permit re-adsorption at relative humidity above 60 %. Moisture verification is performed by ISO 15512:2019 or a calibrated Karl Fischer titrator, not by weight-loss infrared balance alone.

    Storage of unopened bags in an unconditioned warehouse at relative humidity above 60 % for more than 24 h increases the drying load. Bags should be resealed under dry air after partial use; if pellet moisture reaches 1,500 ppm, the drying time must be extended beyond 8 h or the material should be rejected for critical thickness applications.

    On a single-screw extruder with L/D 30:1 to 36:1, REVODE711H is processed with a reverse temperature profile—feed throat at 165–175 °C, compression zone at 185–195 °C, metering zone and adapter at 200–210 °C. The melt temperature at the die must remain below 220 °C; above this threshold, PLA degrades to lactide and acetaldehyde-like volatiles, visible as vacuum-vent plate-out and sheet edge yellowing. On co-rotating twin-screw lines with L/D 44:1, melt temperature is controlled primarily by screw speed rather than barrel set-point; a screw speed increase of 20 % can raise melt temperature by 8–12 °C when die pressure exceeds 80 bar. Barrel temperature alone does not validate the process: melt temperature is measured with an immersion thermocouple at the adapter. Vacuum venting at -0.6 bar gauge or lower is applied after the first mixing zone to remove moisture and volatile degradation products. Between the extruder and the sheet die, a continuous screen changer or breaker plate with 100–150 mesh filtration is used to capture degraded gel particles. Gear pumps are preferred for sheet lines to reduce pressure pulsation; the pump inlet pressure is maintained at 30–50 bar and the die pressure at 80–120 bar.

    Thermal Transitions and Crystallization Kinetics in Unmodified PLLA Sheet

    Differential scanning calorimetry according to ASTM D3418-21 on semicrystalline PLLA typically reveals a glass transition at 55–60 °C, a cold-crystallization exotherm near 100–120 °C, and a melting endotherm at 145–155 °C. REVODE711H, as an extrusion grade, may be nucleated or formulated to accelerate crystallization during sheet formation and thermoforming; however, the exact nucleation package and isothermal crystallization half-time are not published in open grade datasheets. Sheet must pass through the roll stack below the glass transition quickly enough to limit uncontrolled crystallinity, but not so quickly that frozen-in orientation creates dimensional instability. Amorphous PLA sheet typically measures 1.24–1.26 g/cm³ by ISO 1183-1:2019, while heavily crystallized PLA rises toward 1.29 g/cm³. For quality control, haze and heat distortion temperature per ASTM D1525-17e1 are more reliable than density because the density shift is small. Unmodified amorphous PLLA often shows a Vicat A120 temperature near 58–60 °C; nucleated crystallized sheet may exceed 120 °C under ISO 75-2:2020 method B at 0.45 MPa, but this is process-dependent and must be verified.

    Roll-stack temperatures for REVODE711H sheet are typically set between 40 °C and 60 °C on the top roll and 30–40 °C on the lower rolls, with the sheet surface quenched below the glass transition before edge trimming. If the middle roll temperature exceeds 65 °C, the sheet may adhere to the roll or develop contact marks. Edge trim can be ground and returned to the process only after being dried to the same moisture specification as virgin pellets; otherwise the trim introduces additional water into the extruder.

    Compared with an injection-moulding PLA such as a general-purpose 300-series grade, REVODE711H is expected to show a lower melt flow rate and a broader processing window for sheet die lips. Most sheet extrusion PLLA grades are specified at melt mass-flow rates of 2–6 g/10 min under ISO 1133-1:2022 at 210 °C with 2.16 kg; general-purpose injection grades may exceed 15 g/10 min. The lower MFR of REVODE711H, if confirmed on the COA, corresponds to higher melt tension and lower sag in thermoforming. However, MFR alone is not a reliable indicator of melt strength because die swell and extensional viscosity also depend on molecular weight distribution and branching. The 700-series may therefore be tailored with a slightly higher D-lactic acid content or linear chain architecture to slow crystallinity and improve processability. Users should not assume that REVODE711H is a drop-in replacement for another PLA grade based on MFR alone. In contrast, impact-modified PLA compounds containing 10–20 wt% poly(butylene adipate-co-terephthalate) (PBAT) or reactive rubber phases exhibit higher elongation at break but lower tensile modulus; those grades are selected when ISO 527-2:2012 elongation exceeds 50 %. REVODE711H should not be regarded as a high-impact grade unless the COA reports a notched Izod value under ISO 180:2019 above the unmodified PLLA baseline of approximately 3 kJ/m². For rigid thermoformed trays and cups that require stiffness and uniform gauge, this unmodified PLLA is the appropriate portfolio choice. For films requiring low-temperature stretch, selection shifts to PLA copolymers or PBAT blends.

    When Inline Thermoforming Requires Stable Melt Strength at Low Draw Ratios

    In inline thermoforming, two competing mechanisms control the forming stability of REVODE711H sheet: heat-induced chain relaxation and strain-induced crystallization. At surface temperatures above 100 °C, thin sheet may become too fluid for stable bubble pre-stretch; at surface temperatures below 80 °C, the sheet may tear or stress-whiten at plug-assist edges. The forming window for unmodified PLA is often 80–110 °C surface temperature, measured by contact pyrometer at the clamp frame and plug contact points. Gauge uniformity in the finished part is affected by melt orientation in the extruded sheet. If machine-direction thickness variation exceeds ±3 % of nominal gauge, the sheet is rejected before thermoforming because orientation memory causes non-uniform sag. Melt strength also influences the plug-assist settings: a plug with synthetic rubber surface and closed-loop temperature control is used to avoid sticking, and plug speed is kept below 400 mm/s to prevent localized shear heating. Published data for REVODE711H thermoforming settings is limited; the parameters given here are validation starting points for unmodified PLLA sheet, not certified machine recipes.

    For regrind fractions above 30 wt%, the reduction in intrinsic viscosity becomes measurable, and the sheet may exhibit lower tear resistance and increased gel formation at the die lip. Process regrind of REVODE711H can be re-extruded at addition levels up to 30 wt% in most rigid sheet operations, provided that regrind is dried to below 250 ppm moisture and is free of paper labels, silicone release agents, and polyolefin contamination. Intrinsic viscosity is measured by ISO 1628-1:2021 using chloroform or tetrahydrofuran at 30 °C. The use of thermal stabilizer masterbatch is not universally recommended for PLA because stabilizing chemistry can alter crystallization rates and may interfere with compostability certification. REVODE711H should be purged from the extruder with a low-MFR PLA or commercial purging grade when transitioning to polypropylene or polystyrene; residual PLA in a polyolefin stream causes phase separation and surface defects. Conversely, contamination with PVC or PVDC must be avoided because thermal decomposition of chlorinated polymers generates hydrogen chloride, which catalyzes PLA hydrolysis.

    At the finished-article level, compliance must be verified rather than inferred from a resin datasheet. REVODE711H is subject to REACH Regulation 1907/2006 article obligations for substances of very high concern, and to EU RoHS Directive 2011/65/EU if the converted article falls within electrical and electronic equipment scope. Food-contact suitability under (EU) No 10/2011 requires overall migration and specific migration testing on the final package, because conversion conditions and additive packages determine compliance. Industrial compostability is not granted by the resin alone; certification requires EN 13432:2000 or ISO 17088:2021 testing of the finished article. Therefore a resin datasheet claiming “compostable” is insufficient for market claims.